Automotive fastener prints name a material grade, a property class, or both. Carbon and alloy steels such as 1010, 1018, 10B21, 35CrMo, 42CrMo and SCM435 appear often enough to be familiar examples, but they are examples, not a preferred stock list from which a substitute can be chosen. The grade that is written on the current revision is the grade that is quoted. A “similar heading-quality steel” or a grade that is already on the shelf is not a substitute unless the print, or a written change, allows it.
SUNHY reviews the specified grade on bolts, screws and studs, on special nuts and on other made-to-print components, together with the property class and the heat-treatment condition. The notes on material grade and certificates, on property classes and on heat treatment belong beside this one. This article looks at how carbon and alloy grades should be written in an RFQ, and at what is not assumed when the print is silent.
The grade on the revision is the requirement
A complete call-out names the grade or the standard designation, the condition if it is required in the starting material, and any restriction on residual elements, hardenability or a customer material specification. If the print names a property class but is silent on the grade, that is an open item, not a licence to choose a convenient steel that can usually meet the class. If it names a grade but is silent on the class, the mechanical requirements that are actually written — hardness, tensile, or none — are the requirements; a class is not invented.
Equivalent designations in different systems (for example a CrMo grade and an SCM or AISI-style designation) are not treated as interchangeable without a stated equivalence on the print or in an attached specification. A boron steel such as 10B21 is not exchanged for a non-boron carbon steel, or the reverse, just because both can be headed. Those substitutions change hardenability and process windows, and they are process and specification changes, not informal conveniences.
What the grade does and does not decide
The grade, together with the section size and the process, influences whether a part can be cold headed, whether it needs an intermediate anneal, and how it will respond to quench and temper or to case hardening. Those process implications are reviewed, as in the notes on cold heading versus CNC, on annealing and in-process softening and on carburizing and case hardening. They do not authorise a change of grade to make heading easier, and they do not authorise a heat treatment that the print does not require.
Property class, hardness and tensile checks remain as specified, independently of a familiar grade name. A 42CrMo blank is not assumed to be class 12.9, and a 10B21 part is not assumed to be class 9.8 or 10.9, unless the print says so. The inspection evidence that is actually required — hardness, tensile, decarburization, or none of these — is confirmed per order, as already described in the note on hardness and tensile checks.
Certificates, analysis and traceability
Material certificates and any EN 10204 3.1 evidence, ladle or product analysis, and lot traceability are confirmed per order when they are required, not issued automatically in every possible form. If a particular certificate, an IMDS record, or a restricted-substance statement is already decided, name it. A verbal assurance that “it is 35CrMo” is not a substitute for the document the order requires. Those points are developed in the existing notes on material certificates and on order documents.
Incoming identification of the grade, when it is part of the agreed control plan, belongs with the lot, not only with a mill certificate in a file. Spectrometric or other identification checks are used when the order or the control plan requires them, not as an unstated extra on every batch. Packing and labelling should keep that lot identity intact, as in the note on packing, labelling and lot traceability.
Coatings and high-strength conditions
Higher-strength carbon and alloy fasteners often carry a coating and a hydrogen-embrittlement-control requirement. Those conditions stay with the print and with the agreed route; they are not informal extras and they are not assumed from the grade name alone. The existing coatings note describes that control. A change of grade that is offered “because it plates more easily” is still a specification change and is not made on the shop floor.
Stainless grades, when they are specified, are a different family and are not a substitute for a carbon or alloy print, or the reverse. They are discussed in the note on stainless fasteners in 304 (A2), 316 (A4) and 410. Mixed notes on a drawing — an alloy steel in the title block and a stainless finish in a call-out, for example — are flagged as conflicts, not resolved by a preferred stock.
What to write in the RFQ
Quote the material grade or customer material specification, the property class or the mechanical requirements, any starting-condition or hardenability note, the heat-treatment and coating requirements, the documents you need (including EN 10204 3.1, PPAP or IMDS if required), the volume and the rest of the part as they appear on the current revision. Send the print with the request form, not a request to pick a steel from a preferred list.
Send the print. The scope is confirmed before quote.
Email the current drawing revision, or use the request form. Unspecified points will be flagged before production rather than assumed.
This article is a capability and commercial note. It is not a certificate, a dimensional data book, or evidence of customer approval. Catalogue type codes and example grades do not replace the customer’s item number, material specification or drawing revision.