The coating on a high-strength fastener is taken from the customer’s drawing and confirmed with the order. It is not chosen from a photograph, and it is not a generic “zinc finish” when the print names a system. This note is for purchasing and supplier-quality engineers who need the coating, the friction condition and any hydrogen-embrittlement control to be visible in the RFQ, so that the process can be set before production rather than assumed later.
Finishes that can be reviewed on automotive fasteners include trivalent zinc, zinc-nickel, zinc-flake systems, passivation, and a wax or topcoat used to hold a specified friction window, when those systems are called up on the print. The same rule applies to carbon-steel fitting parts that are zinc plated when that is specified. Colour in a catalogue model does not represent the specified material or finish.
Name the system, not a colour
Write the coating as it appears on the drawing: the system, any thickness or class, the passivation or topcoat, and a friction or torque-tension window if one is specified. Zinc, zinc-nickel and zinc-flake coatings are examples of systems that are reviewed when the print calls them up. Zinc-flake systems such as Geomet or Dacromet are cited on the quality page as examples of coating types; they are not a preferred list, and they are not substituted for a different system named on the drawing.
Corrosion-test hours — salt-spray or otherwise — are treated as typical buyer-specified values, or as a process target for the system named on the print. They are not published here as a performance claim, and they are not a guarantee on every lot. If a test duration, a method or an acceptance limit is already decided, it belongs in the RFQ and must come from the drawing or the customer specification, not from a catalogue assumption.
High-strength parts and hydrogen embrittlement
Hydrogen embrittlement is a genuine process risk on high-strength steel parts, particularly where an electrolytic coating or pretreatment is used. It is not a reason to overstate the risk, and it is not a reason to change the specified coating without agreement. When property class 10.9, 12.9 or an equivalent high-strength condition is specified, pretreatment, any electrolytic step, baking and the overall coating process require review.
Zinc-flake coatings are non-electrolytic, which is often a reason for reviewing them on high-strength parts when the print allows that system. The method actually used — including any bake, hold time or alternative process — is agreed in the quotation against the drawing and the specification. A bake cycle is not invented here as a standard inclusion, and a change of coating system is not made in the shop to avoid a control step. If a hydrogen-embrittlement test or a documented bake is required, state that in the enquiry.
Friction, torque and the rest of the fastener
A wax or topcoat is often specified to hold a friction window, not as a decorative layer. If a coefficient-of-friction range, a k-factor or a torque-tension requirement is on the print or in the customer specification, it should be in the RFQ. The coating system and the lubricant or topcoat are reviewed together, because a change in either can move the assembly result. Those values are taken from the specified system; they are not assumed from a previous lot or from a catalogue finish.
The coating review also has to see the rest of the part: property class, heat-treatment condition, thread class, and any surfaces that must remain uncoated or masked. A heading or machining route that is still open will be flagged, because the sequence of heat treatment, coating and thread rolling or cutting affects both hydrogen-embrittlement control and the final gauge condition.
Thread condition after coating
A coating changes the thread. If the finished fastener must gauge after coating, that condition has to be in the inspection plan; it is not applied automatically to every lot. Go / no-go gauging after coating, and any measured pitch-diameter requirement, should be written in the RFQ. Thread standards, pitch and gauging sets out the same point for metric and inch threads.
What belongs in the RFQ
Name the coating system and any thickness or class, the passivation or topcoat, the friction window if one applies, the gauging condition after coating, and any hydrogen-embrittlement control or test that the specification requires. If only an uncoated condition is to be gauged, say so. Material, property class and heat-treatment condition should be stated as they appear on the drawing, because they govern how the coating process is reviewed.
Send the current revision with the request form or to anna@sunhyings.com. Related notes cover what to include in a made-to-print RFQ, materials and finishes on gas-equipment prints, and documents confirmed per order.
This article is a capability and commercial note. It is not a certificate, a dimensional data book, or evidence of customer approval. Catalogue type codes and example grades do not replace the customer’s item number, material specification or drawing revision.