When a made-to-print fastener or component is coated, thickness is inspected as the specification requires. The method — magnetic induction, X-ray fluorescence, microsection, or another named method — and the location of the readings are taken from the print, the coating specification, or the written order. They are not taken from a shop habit of measuring on the most convenient flat. Thickness on threads, heads, shanks, recesses and internal surfaces can differ, and those differences matter for fit and function. Related comments already appear in the notes on Coating thickness and thread class and on Coatings for high-strength fasteners and hydrogen-embrittlement control.
What has to be named
A complete instruction names the coating system, the required thickness or thickness range, the method, the number and location of readings, and whether values are taken before or after any topcoat or lubricant. If a local minimum on a thread or a head is required, that location should be stated. “Thickness as usual” is not complete. Named flake systems and electroplated systems are reviewed only as the print calls them up, as in the notes on Zinc-flake systems as specified and on Zinc-nickel and electroplated zinc.
The instrument and any required agreement or calibration check belong with the method, as in the note on Measurement system and gauge agreement. A microsection that destroys a part is a different plan from a non-destructive reading; if a section is already required, it should be named so that sample pieces can be planned.
Threads, masking and interference with gauges
Thickness on a thread affects gauge fit and may be limited by the specified thread class after coating. Those limits are taken from the print and are not guessed from a catalogue class. Internal threads, recesses and masked areas follow the masking and internal-coating notes already on this site. A thickness reading on a washer face does not by itself represent a thread flank, and a reading on a masked zone is not evidence of the coated zone.
Appearance, adhesion and other coating checks are separate characteristics. A correct thickness is not a substitute for an adhesion or appearance requirement, as in the note on Appearance, adhesion and coating inspection. Salt-spray hours, when they are specified, remain a specification item and are not treated as a published site result, as in the note on Salt-spray hours follow the specification.
Hydrogen-embrittlement relief and certificates
On high-strength parts, any required hydrogen-embrittlement relief remains confirmed per order when it applies, as already stated in the coating notes. Certificates and any EN 10204 3.1 evidence of the coating, including thickness records when they are required, are confirmed per order. IMDS or other substance data, when requested, have to reflect the actual coating system, not a generic family name.
Route, first article, conflicts and volume
The coating source and the measurement method are part of the agreed route. A change of source is a process change, as in the note on A change of subcontractor is a process change. First-article inspection, when required, should report thickness at the specified locations using the production-intent method, as in the note on First-article inspection on made-to-print parts. A print that names a thickness and a thread class that cannot be held together, or that asks for a method the geometry cannot accept, is flagged. Volume belongs in the enquiry because the number of readings and whether a section is justified depend on quantity and risk.
Maps, curves and awkward geometry
Thickness is rarely uniform on a headed bolt, a recessed screw, a weld-nut body or a small stub. A map or a table of locations — head, shank, thread, recess, internal wall — should follow the specification when it gives one, and should be proposed honestly when it does not. Edge effect, curvature and a deep recess can mislead some instruments; those limits are respected rather than hidden by choosing an easy flat that the specification does not recognise.
A thickness “curve” promised from a short prototype run is not a substitute for the specified locations in series. If the racking or the barrel load will change with volume, the first-article thickness map should be taken under the serial condition, or the difference should be visible in the quotation. Related bath or flake-process changes remain process changes, even when the target thickness is unchanged. The measurement plan travels with the process; it is not a once-only laboratory favour.
Local thickness also matters where a later gauge, a nut, or a mating face will sit. A heavy build on a flange that will be clamped, or a thin patch beside a mask line, can be out of specification even when an average of convenient flats looks acceptable. Those local conditions are inspected when the specification names them, and they are flagged when the specification is silent but the conflict is visible on the part or the drawing. Thickness evidence is evidence of the coating as applied; it is not a friction-class result and it is not a salt-spray certificate.
What to send with the RFQ
Send the current drawing revision, the coating specification, material, finish and volume. If a particular method, location map, or first-article thickness record is already required, say so. Unspecified points will be flagged before production rather than assumed.
This article is a capability and commercial note. It is not a certificate, a dimensional data book, or evidence of customer approval. Catalogue type codes and example grades do not replace the customer’s item number, material specification or drawing revision.